Armox® 500T

Loading component...

General Product Description

Mechanical Properties

Thickness
(mmin)
Thickness
(mmin)
3.0 - 80.01.2 - 31.5
Hardness
(HBW)
480 - 540
Yield strength Rp0.2
(min MPa)
1250
Tensile strength Rm
(MPa)
1450 - 1750
Elongation A5
(min %)
8

Impact Properties

Thickness
(mmin)
Thickness
(mmin)
3.0 - 80.01.2 - 31.5

Average of three tests. Single value min. 70% of specified average. For plate thicknesses under 12 mm sub-size Charpy-V specimen are used. The specified minimum value is then propotional to the specimen cross-section.

 

 

Chemical Composition (heat analysis)

C *)
(max %)
C *)
(max %)
0.32
Si *)
(max %)
0.40
Mn*)
(max %)
1.20
P
(max %)
0.010
S
(max %)
0.003
Cr*)
(max %)
1.0
Ni*)
(max %)
1.80
Mo*)
(max %)
0.70
B*)
(max %)
0.005

The steel is grain-refined. *) Intentional alloying elements.

For plate thicknesses >70 mm Cr ≤ 1.5 and Ni ≤3.5

 

Tolerances

Thickness

Length and Width

Shape

Flatness

Surface Properties

Delivery Conditions